Material Notes:
FeaturesBasic type PA 6 for injection moulding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, hobby tools, toys. Delivered in the natural and in the full RAL color scale.Application: Injection MouldingInformation Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
STN 64 0111
Linear Mold Shrinkage 0.018 cm/cm
0.018 in/in
STN 64 0808
Linear Mold Shrinkage, Transverse 0.0183 cm/cm
0.0183 in/in
STN 64 0808
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 85.0 MPa
12300 psi
STN EN ISO 527-2
Elongation at Break 3.5 %
3.5 %
STN EN ISO 527-2
Tensile Modulus 3.10 GPa
450 ksi
STN EN ISO 527-2
Flexural Strength 115 MPa
16700 psi
STN EN ISO 178
Flexural Modulus 2.70 GPa
392 ksi
STN EN ISO 178
Charpy Impact Unnotched 8.00 J/cm²

@Temperature -20.0 °C
38.1 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
12.0 J/cm²

@Temperature 23.0 °C
57.1 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Charpy Impact, Notched 0.150 J/cm²

@Temperature -20.0 °C
0.714 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
0.160 J/cm²

@Temperature 23.0 °C
0.761 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
DSC; STN EN ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
STN EN ISO 75/A
Vicat Softening Point 190 °C
374 °F
B; STN EN ISO 306
Flammability, UL94 HB
HB
Glow Wire Test 960 °C
1760 °F
STN IEC 60695-2-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
STN IEC 60093
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
STN IEC 60093
Dielectric Strength 18.0 kV/mm
457 kV/in
STN IEC 60243
Comparative Tracking Index 600 V
600 V
STN 34 6468
Processing Properties Metric English Comments
Melt Temperature 250 - 270 °C
482 - 518 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour
Moisture Content 0.15 %
0.15 %
STN EN ISO 960
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi