Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Riblene® MQ 10 Low Density Polyethylene - Injection Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Riblene® MQ 10 Low Density Polyethylene - Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Riblene MQ 10 is a good fluidity low density polyethylene resin (LDPE).Parts made with Riblene MQ 10 are characterized by a high flexibility.Main Applications: Riblene MQ 10 is suitable for injection molding and compound applications. Riblene MQ 10 is recommended for stoppers, closures and low thickness articles.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.918 g/cc
0.918 g/cc
ISO 1183
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 190 °C
15 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 46
46
ISO 868/A
Tensile Strength, Yield 10.0 MPa
1450 psi
ISO 527
Flexural Modulus 0.120 GPa
17.4 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 108 °C
226 °F
Internal method
Vicat Softening Point 84.0 °C

@Load 1.00 kg
183 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -40.0 °C
<= -40.0 °F
ASTM D746