Material Notes:
Resinlab™ EP1026HP is a high performance fast setting epoxy adhesive designed for bonding metals, ceramics, glass and most plastics. This product gives good resistance to water salt spray, inorganic acids and bases and most organic solvents.Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
Part B; TM R050-16
1.15 g/cc
1.15 g/cc
Mixed; TM R050-16
1.16 g/cc
1.16 g/cc
Part A; TM R050-16
Water Absorption 1.47 %

@Time 86400 sec
1.47 %

@Time 24.0 hour
TM R050-35
Viscosity 10000 cP
10000 cP
Part A, RVT, #5, 2.5 rpm; TM R050-12
12500 cP
12500 cP
Mixed; TM R050-12
15000 cP
15000 cP
Part B, RVT, #5, 2.5 rpm; TM R050-12
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
TM R050-17
Tensile Strength at Break 22.8 MPa
3300 psi
TM R050-36
Tensile Strength, Ultimate 22.8 MPa
3300 psi
TM R050-36
Tensile Strength, Yield 17.2 MPa
2500 psi
TM R050-36
Elongation at Break 20 - 30 %
20 - 30 %
TM R050-36
Tensile Modulus 1.38 GPa
200 ksi
TM R050-36
Compressive Yield Strength 31.0 MPa
4500 psi
TM R050-38
Compressive Strength >= 193 MPa
>= 28000 psi
Ultimate; TM R050-38
>= 193 MPa
>= 28000 psi
Break; TM R050-38
Compressive Modulus 1.38 GPa
200 ksi
TM R050-38
Adhesive Bond Strength 24.1 MPa
3500 psi
Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37
Peel Strength 2.63 kN/m
15.0 pli
Al to Al
Thermal Properties Metric English Comments
CTE, linear 55.0 µm/m-°C
30.6 µin/in-°F
Thermal Conductivity 0.140 W/m-K
0.972 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Glass Transition Temp, Tg 30.0 °C
86.0 °F
TM R050-25
Electrical Properties Metric English Comments
Volume Resistivity 8.00e+14 ohm-cm
8.00e+14 ohm-cm
Dielectric Constant 4.5

@Frequency 100 Hz,
Temperature 25.0 °C
4.5

@Frequency 100 Hz,
Temperature 77.0 °F
Dielectric Strength 17.3 kV/mm
440 kV/in
Processing Properties Metric English Comments
Pot Life 3.0 - 5.0 min
3.0 - 5.0 min
Mass: 50g; TM R050-19
Descriptive Properties Value Comments
Color Off-White
Mix Ratio 1:1
Weight and Volume