Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Resistalloy International Fecralloy™ 134 Electrical Resistance Steel

Category Metal , Electronic/Magnetic Alloy , Ferrous Metal , Stainless Steel , Superalloy
Manufacturer Resistalloy International Limited
Trade Name Fecralloy™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resistalloy International Fecralloy™ 134 Electrical Resistance Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ferritic stainless steel with aluminum. Available as wire and strip. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of atmospheres. "Fecralloy"** an Fe-Cr-Al steel containing "yttrium" is a versatile alloy and is suitable for use over a wide range up to 1300°C. The "yttrium" is the key to its longer high temperature life, having greater oxidation resistance and form stability over other resistance alloys.**"Fecralloy" is the registered trademark of the UK Atomic Energy Authority (Now AEA Technology, Harwell). Information provided by Resistalloy International Limited.
Physical Properties Metric English Comments
Density 7.28 g/cc
0.263 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 230
230
Tensile Strength, Ultimate 750 MPa
109000 psi
30.0 MPa

@Temperature 900 °C
4350 psi

@Temperature 1650 °F
Tensile Strength, Yield 550 MPa
79800 psi
Elongation at Break 16 - 20 %

@Thickness 50.0 mm
16 - 20 %

@Thickness 1.97 in
Thermal Properties Metric English Comments
CTE, linear 11.0 µm/m-°C

@Temperature 20.0 - 250 °C
6.11 µin/in-°F

@Temperature 68.0 - 482 °F
12.0 µm/m-°C

@Temperature 20.0 - 500 °C
6.67 µin/in-°F

@Temperature 68.0 - 932 °F
15.0 µm/m-°C

@Temperature 20.0 - 1000 °C
8.33 µin/in-°F

@Temperature 68.0 - 1830 °F
Specific Heat Capacity 0.480 J/g-°C
0.115 BTU/lb-°F
Thermal Conductivity 16.0 W/m-K
111 BTU-in/hr-ft²-°F
Melting Point 1500 °C
2730 °F
Maximum Service Temperature, Air 1100 °C
2010 °F
Optical Properties Metric English Comments
Emissivity (0-1) 0.70
0.70
Fully Oxidized
Component Elements Properties Metric English Comments
Aluminum, Al 4.3 %
4.3 %
Chromium, Cr 15 %
15 %
Iron, Fe 81 %
81 %
As remainder
Electrical Properties Metric English Comments
Electrical Resistivity 0.000126 ohm-cm
0.000126 ohm-cm
Temperature Factor is 1.10 at 800°C (1470°F). Temperature Factor is 1.11 at 1000°C (1830°F).
Curie Temperature 600 °C
1110 °F