SABIC Innovative Plastics Cycoloy® EFX830ME PC

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Cycoloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Cycoloy® EFX830ME PC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame retardant modified PC blend using non-brominated and non-chlorinated flame retardant systems, offering metallic / sparkle look with minimal flow line visibilityThis data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.10 %
0.10 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.25 %

@Temperature 23.0 °C
0.25 %

@Temperature 73.4 °F
ISO 62
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 260 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 500 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.0 MPa
8700 psi
50 mm/min; ISO 527
Tensile Strength, Yield 62.0 MPa
8990 psi
50 mm/min; ISO 527
Elongation at Break 5.0 %
5.0 %
50 mm/min; ISO 527
Elongation at Yield 4.0 %
4.0 %
50 mm/min; ISO 527
Tensile Modulus 2.70 GPa
392 ksi
1 mm/min; ISO 527
Flexural Yield Strength 97.0 MPa
14100 psi
2 mm/min; ISO 178
Flexural Modulus 2.40 GPa
348 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
6.00 kJ/m²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 31.0 kJ/m²

@Temperature 23.0 °C
14.8 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C
187 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Vicat Softening Point 103 °C
217 °F
Rate B/50; ISO 306
105 °C
221 °F
Rate B/120; ISO 306
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
ASTM D 257
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
ASTM D 257
Dielectric Constant 2.9

@Frequency 50.0 - 60.0 Hz
2.9

@Frequency 50.0 - 60.0 Hz
ASTM D 150
2.9

@Frequency 1.00e+6 Hz
2.9

@Frequency 1.00e+6 Hz
ASTM D 150
Dissipation Factor 0.0040

@Frequency 1.00e+6 Hz
0.0040

@Frequency 1.00e+6 Hz
ASTM D 150
0.020

@Frequency 50.0 - 60.0 Hz
0.020

@Frequency 50.0 - 60.0 Hz
ASTM D 150