SABIC Innovative Plastics LNP STAT-KON MD000I PP (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON MD000I PP (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Stat-kon* MD000I is a compound based on Polypropylene resin. Added features of this material include: Electrically Conductive, High Impact.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 16.0 MPa
2320 psi
5 mm/min; ISO 527
Tensile Strength, Yield 27.0 MPa
3920 psi
5 mm/min; ISO 527
Elongation at Break 24 %
24 %
5 mm/min; ISO 527
Elongation at Yield 4.3 %
4.3 %
5 mm/min; ISO 527
Flexural Strength 40.0 MPa
5800 psi
2 mm/min; ISO 178
Flexural Modulus 1.60 GPa
232 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 60.0 kJ/m²
28.6 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 130 µm/m-°C

@Temperature 23.0 - 60.0 °C
72.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 148 µm/m-°C

@Temperature 23.0 - 60.0 °C
82.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 61.0 °C
142 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D257