SABIC Innovative Plastics NORYL RN0401 PPE+PS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL RN0401 PPE+PS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Noryl RN0401 resin is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether blend comprising at least 20% PCR content. Available in black only.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Density 1.11 g/cc
0.0401 lb/in³
ISO 1183
Melt Flow 30 g/10 min

@Load 5.00 kg,
Temperature 260 °C
30 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Melt Index of Compound 30 g/10 min

@Load 5.00 kg,
Temperature 260 °C
30 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.0 MPa
5080 psi
50 mm/min; ISO 527
40.0 MPa
5800 psi
Type I, 50 mm/min; ASTM D638
Tensile Strength, Yield 50.0 MPa
7250 psi
50 mm/min; ISO 527
55.0 MPa
7980 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 15 %
15 %
Type I, 50 mm/min; ASTM D638
15 %
15 %
50 mm/min; ISO 527
Elongation at Yield 3.0 %
3.0 %
Type I, 50 mm/min; ASTM D638
3.0 %
3.0 %
50 mm/min; ISO 527
Tensile Modulus 2.10 GPa
305 ksi
5 mm/min; ASTM D638
2.20 GPa
319 ksi
1 mm/min; ISO 527
Flexural Yield Strength 75.0 MPa
10900 psi
2 mm/min; ISO 178
80.0 MPa
11600 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.30 GPa
334 ksi
2 mm/min; ISO 178
2.50 GPa
363 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
70.0 °C

@Thickness 3.20 mm
158 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 94.0 °C
201 °F
Rate B/120; ISO 306
UL RTI, Electrical 65.0 °C
149 °F
UL 746B
UL RTI, Mechanical with Impact 65.0 °C
149 °F
UL 746B
UL RTI, Mechanical without Impact 65.0 °C
149 °F
UL 746B
Flammability, UL94 V-0

@Thickness 2.00 mm
V-0

@Thickness 0.0787 in
UL 94 by SABIC-IP
Electrical Properties Metric English Comments
Dielectric Strength 25.0 kV/mm

@Thickness 3.20 mm
635 kV/in

@Thickness 0.126 in
in oil; ASTM D149
Arc Resistance 0.00 - 60 sec
0.00 - 60 sec
Tungsten; ASTM D495
Comparative Tracking Index 250 - 400 V
250 - 400 V
UL 746A
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A