SABIC Innovative Plastics NORYL WCA901 PPE-TPE (Asia Pacific)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL WCA901 PPE-TPE (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL 1581. Good processing performance by using standard extrusion equipment. UL1581 tests conducted on 2.0 mm wire with 0.12 mm x 20 stranded copper conductor.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Melt Flow 10 g/10 min

@Load 10.0 kg,
Temperature 250 °C
10 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 91
91
30S reading; ASTM D2240
Tensile Strength at Break 22.0 MPa
3190 psi
50 mm/min; ISO 527
23.0 MPa
3340 psi
Type I, 50 mm/min; ASTM D638
26.0 MPa
3770 psi
UL 1581
27.0 MPa
3920 psi
after 7days @136°C; UL 1581
Elongation at Break 95 %
95 %
50 mm/min; ISO 527
110 %
110 %
Type I, 50 mm/min; ASTM D638
127 %
127 %
after 7days @136°C; UL 1581
190 %
190 %
UL 1581
Flexural Modulus 0.390 GPa
56.6 ksi
12.5 mm/min, 100 mm span; ASTM D790
0.390 GPa
56.6 ksi
12.5 mm/min; ISO 178
Tear Strength 13.0 kN/m
74.2 pli
ISO 6383
Heat Distortion 15 %

@Load 0.250 kg,
Temperature 121 °C
15 %

@Load 0.551 lb,
Temperature 250 °F
UL 1581
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
UL temperature rating; UL 1581
Brittleness Temperature <= -40.0 °C
<= -40.0 °F
ASTM D746
Flammability, UL94 V-0

@Thickness 6.00 mm
V-0

@Thickness 0.236 in
UL 94 by SABIC-IP
Oxygen Index 27 %
27 %
ISO 4589
Glow Wire Test 775 °C
1430 °F
IEC 60695-2-13
850 °C

@Thickness 3.00 mm
1560 °F

@Thickness 0.118 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 5.10e+15 ohm-cm
5.10e+15 ohm-cm
ASTM D257
Surface Resistance 4.20e+16 ohm
4.20e+16 ohm
ASTM D257
Dielectric Constant 2.7

@Frequency 1.00e+6 Hz
2.7

@Frequency 1.00e+6 Hz
IEC 60250
Dissipation Factor 0.0040

@Frequency 1.00e+6 Hz
0.0040

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
VW-1 Pass
UL 1581