Material Notes:
Description: DEXFLEX® E756 thermoplastic olefinic elastomer (TPO) is designed for extruded automotive air-bag covers. This material provides excellent rigidity, durability and low-temperature toughness. This material is colorable and can be supplies with or without UV stabilizers. Applications: Passenger and roof-mounted air-bag covers that require stiffness and that operate in temperatures ranging from -40°C to 104°C Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ISO 1183
Melt Flow 0.60 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.60 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
ISO 868
Tensile Strength, Yield 14.0 MPa
2030 psi
ISO 527-1
Flexural Modulus 0.410 GPa
59.5 ksi
ISO 178
Izod Impact, Notched 0.801 J/cm

@Temperature -40.0 °C
1.50 ft-lb/in

@Temperature -40.0 °F
NB; ISO 180
Impact Test 33.0 J
24.3 ft-lb
multiaxial, ultimate energy, 8.9 m/s; ISO 6603-2
Multi-axial Impact @ -30°C Total Energy 54.9 J
40.5 ft-lb
8.9 m/s; ISO 6603-2
Thermal Properties Metric English Comments
CTE, linear 71.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
39.4 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 45.0 °C
113 °F
ISO 75.1
Deflection Temperature at 1.8 MPa (264 psi) 37.8 °C
100 °F
ISO 75.1