Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber

Category Polymer , Thermoplastic , Polyketone , Polyaryletherketone (PAEK), Glass Fiber Filled
Manufacturer Solvay Specialty Polymers
Trade Name AvaSpire®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AvaSpire® AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical strength and stiffness than unfilled AV-650 resin. This material can be repeatedly exposed to harsh chemicals and prolonged steam sterilization cycles without any significant loss of properties. Potential applications for this resin include orthopedic and dental instruments, surgical power tool battery housings and other devices and components requiring a combination of high temperature performance and high environmental resistance. AvaSpire® AV-650 GF30 can be easily processed by typical injection molding and extrusion methods using standard equipment.Features: Fatigue Resistant; Flame Retardant; Good Chemical Resistance; Good Dimensional Stability; High Heat Resistance; High Stiffness; High StrengthUses: Medical/Healthcare Applications; Oil/Gas Applications; Power/Other ToolsAdditional Properties: Water Absorption - ASTM D570 0.40 %Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ASTM D792
Filler Content 30 %
30 %
Glass Fiber
Water Absorption 0.20 %

@Time 86400 sec
0.20 %

@Time 24.0 hour
ISO 62
Viscosity 410000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
410000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt Viscosity; ASTM D3835
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm

@Thickness 3.18 mm
0.0010 - 0.0030 in/in

@Thickness 0.125 in
Linear Mold Shrinkage, Transverse 0.0080 - 0.010 cm/cm

@Thickness 3.18 mm
0.0080 - 0.010 in/in

@Thickness 0.125 in
ASTM D955
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 400 °C
15 g/10 min

@Load 4.76 lb,
Temperature 752 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 100
100
ASTM D785
Tensile Strength 142 MPa
20600 psi
ASTM D638
Tensile Strength, Yield 165 MPa
23900 psi
5 mm/min, Type 1A; ISO 527-2
Elongation at Break 2.6 %
2.6 %
Type 1A, 5 mm/min; ISO 527-2
2.6 %
2.6 %
5 mm/min; ASTM D638
Tensile Modulus 10.1 GPa
1460 ksi
ASTM D638
10.5 GPa
1520 ksi
ISO 527-2
Flexural Strength 221 MPa
32100 psi
ASTM D790
240 MPa
34800 psi
ISO 178
Flexural Modulus 9.00 GPa
1310 ksi
ASTM D790
9.80 GPa
1420 ksi
ISO 178
Compressive Strength 163 MPa
23600 psi
ASTM D695
Shear Strength 80.8 MPa
11700 psi
ASTM D732
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
Izod Impact, Unnotched 9.60 J/cm
18.0 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
ISO 180
Izod Impact, Unnotched (ISO) 69.0 kJ/m²
32.8 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
10.6 µin/in-°F

@Temperature -58.0 - 122 °F
1
Specific Heat Capacity 1.29 J/g-°C

@Temperature 50.0 °C
0.308 BTU/lb-°F

@Temperature 122 °F
ASTM C351
1.67 J/g-°C

@Temperature 200 °C
0.399 BTU/lb-°F

@Temperature 392 °F
ASTM C351
Thermal Conductivity 0.290 W/m-K
2.01 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 340 °C
644 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 209 °C

@Thickness 3.20 mm
408 °F

@Thickness 0.126 in
Annealed; ASTM D648
Glass Transition Temp, Tg 158 °C
316 °F
DSC
Flammability, UL94 V-0

@Thickness 0.800 - 1.60 mm
V-0

@Thickness 0.0315 - 0.0630 in
Electrical Properties Metric English Comments
Dielectric Constant 3.6

@Frequency 1.00e+6 Hz
3.6

@Frequency 1.00e+6 Hz
ASTM D150
3.65

@Frequency 60.0 Hz
3.65

@Frequency 60.0 Hz
ASTM D150
3.66

@Frequency 1000 Hz
3.66

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 14.0 kV/mm

@Thickness 3.18 mm
356 kV/in

@Thickness 0.125 in
ASTM D149
Dissipation Factor 0.00

@Frequency 1000 Hz
0.00

@Frequency 1000 Hz
ASTM D150
0.0020

@Frequency 60.0 Hz
0.0020

@Frequency 60.0 Hz
ASTM D150
0.0050

@Frequency 1.00e+6 Hz
0.0050

@Frequency 1.00e+6 Hz
ASTM D150
Processing Properties Metric English Comments
Rear Barrel Temperature 365 °C
689 °F
Middle Barrel Temperature 370 °C
698 °F
Front Barrel Temperature 375 °C
707 °F
Nozzle Temperature 380 °C
716 °F
Melt Temperature 365 - 390 °C
689 - 734 °F
Mold Temperature 150 - 180 °C
302 - 356 °F
Drying Temperature 150 °C

@Time 14400 sec
302 °F

@Time 4.00 hour
Descriptive Properties Value Comments
Agency Ratings FAA FAR 25.853a
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Beige
Form Pellets
Injection Rate Fast
Processing Technique Injection Molding; Machining; Profile Extrusion
Screw Compression Ratio 2.0:1.0 to 3.0:1.0