Polymer Property : Glass Transition Temp, Tg = 316 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 158 °C
316 °F
ASTM D3418
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better dimensiona..
Glass Transition Temp, Tg 158 °C
316 °F
ASTM D3418
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 resin. ..
Glass Transition Temp, Tg 158 °C
316 °F
ASTM D3418
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stability..
Glass Transition Temp, Tg 158 °C
316 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gr..
Glass Transition Temp, Tg 158 °C
316 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gra..
Glass Transition Temp, Tg 158 °C
316 °F
DSC
Solvay Specialty Polymers Ajedium™ Films -- AvaSpire® AV-630 Polyaryletherketone (PAEK)
AvaSpire® AV-630 PAEK film is a unique thermoplastic film that is characterized by a distinct combination of properties, which include strength, ductility, fatigue resistance, high purity and exc..
Glass Transition Temp, Tg 158 °C
316 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire® AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This r..
Glass Transition Temp, Tg 158 °C
316 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK)
AvaSpire® AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. ..
Glass Transition Temp, Tg 158 °C
316 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK)
AvaSpire® AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (..
Glass Transition Temp, Tg 158 °C
316 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical streng..
Glass Transition Temp, Tg 158 °C
316 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better di..
Glass Transition Temp, Tg 158 °C
316 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 res..
Glass Transition Temp, Tg 158 °C
316 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)
AvaSpire® AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than Ava..
Glass Transition Temp, Tg 158 °C
316 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparabl..
Glass Transition Temp, Tg 158 °C
316 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable..
Glass Transition Temp, Tg 158 °C
316 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK)
AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stabi..
Glass Transition Temp, Tg 158 °C
316 °F
10°C/min; ISO 11357-1,-2,-3
Topas Advanced Polymers TOPAS® 6015S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 6015S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma..
Glass Transition Temp, Tg 158 °C
316 °F
ASTM D3418
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. The ..
Glass Transition Temp, Tg 158 °C
316 °F
ASTM D3418
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This resin ret..
Glass Transition Temp, Tg 158 °C
316 °F
ASTM D3418
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (5 mi..
Glass Transition Temp, Tg 158 °C
316 °F
ASTM D3418
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical strength a..
Glass Transition Temp, Tg 158 °C
316 °F
ASTM E 1356
Solvay Specialty Polymers Parmax® 1200 Self-Reinforcing Polyethersulfone  (discontinued **)
PARMAX 1200 self-reinforcing polymer (SRP) is an ultra-high performance amorphous, melt-processable engineering thermoplastic. The unique properties of this material are due primarily to the inheren..
Glass Transition Temp, Tg 158 °C
316 °F
ASTM D3418
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than AvaSpir..