Techmer ES HiFill® PA6 GF/M15 A1 BK 15% Glass/Mineral Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced , Nylon 6, Heat Stabilized
Manufacturer Techmer ES
Trade Name HiFill®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PA6 GF/M15 A1 BK 15% Glass/Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 15% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized Appearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Water Absorption 0.85 %

@Time 86400 sec
0.85 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.015 cm/cm

@Thickness 3.17 mm
0.015 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 75.8 MPa
11000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 117 MPa
17000 psi
ASTM D790
Flexural Modulus 2.83 GPa
410 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm

@Thickness 3.17 mm
1.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 52.2 µm/m-°C
29.0 µin/in-°F
ASTM D696
Melting Point 216 °C
420 °F
Deflection Temperature at 0.46 MPa (66 psi) 199 °C
390 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
270 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+14 ohm-cm
3.00e+14 ohm-cm
ASTM D257
Dielectric Strength 20.5 kV/mm
520 kV/in
Method A (Short-Time); ASTM D149
Copyright © lookpolymers.com All Rights Reserved