Material Notes:
TRA-BOND FDA-8 EPOXY ADHESIVE is a low viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Administration (FDA) Chapter 1, Sub Part B, Sections 175.105 and 175.300. This two-part amber adhesive is easily mixed, used and cured at room temperature for bonding, laminating and repair applications by manufacturers of food preparation, processing and packaging equipment, and by manufacturers of catheters, hearing aids, dental products and other biomedical instruments and devices. TRA-BOND FDA-8 EPOXY ADHESIVE is an effective electrical insulator, and it provides low permeability to gases and vapors, and good resistance to water, weather, galvanic action, to petroleum solvents, lubricants and fuels, to mild acids and alkalis, and to many other organic and inorganic compounds. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
Mixed
Solids Content 100 %
100 %
Reactive Solids Content
Viscosity 1500 cP

@Temperature 25.0 °C
1500 cP

@Temperature 77.0 °F
After mixing
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
Thermal Properties Metric English Comments
CTE, linear 53.0 µm/m-°C

@Temperature 20.0 °C
29.4 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 145 °C
293 °F
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Dielectric Constant 3.35

@Frequency 1000 Hz
3.35

@Frequency 1000 Hz
Dielectric Strength 16.1 kV/mm
410 kV/in
Dissipation Factor 0.020

@Frequency 1000 Hz
0.020

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 65.0 °C
4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 45 min
45 min
Descriptive Properties Value Comments
Color Amber
Mix Ratio, parts by weight 100/100
Resin/Hardener
Thixotropic Index 1