Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tra-Con Tra-Cast FS330 Fire Retardant Long Pot Life Epoxy Casting Compound

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy, Thermally Conductive
Manufacturer Tra-Con, Inc.
Trade Name Tra-Cast
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Cast FS330 Fire Retardant Long Pot Life Epoxy Casting Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-CAST FS330 is a low viscosity, long pot life, thermally conductive casting compound which passes UL 94 V-O. It is recommended for rigid potting, laminating, transformer encapsulating, filament winding and coil embedding applications where a desirable combination of superior mechanical and electrical properties plus fire retardancy and room temperature curing is required. This easy-to-use epoxy system has a low coefficient of thermal expansion, and exhibits excellent wetting and adhesion to most electronic and aerospace-industry materials (metals, glass products, ceramics, industrial laminates and many rigid plastics). Fully cured TRA-CAST FS330 is a durable electrical insulator, dimensionally stable over a wide temperature range, and is resistant to moisture, gases petroleum lubricants and fuels, salts, many mild acids and alkalis, and other organic and inorganic compounds. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.60 g/cc
1.60 g/cc
Mixed
Solids Content 100 %
100 %
Reactive Solids Content
Viscosity 4000 cP

@Temperature 25.0 °C
4000 cP

@Temperature 77.0 °F
After mixing
Mechanical Properties Metric English Comments
Hardness, Shore D 78
78
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Processing Properties Metric English Comments
Cure Time 360 min
6.00 hour
4 hrs @ 25°C + 2 hrs @ 65°C
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 180 min
180 min
Descriptive Properties Value Comments
Color Black
Mix Ratio, parts by weight 100/15
Resin/Hardener