Material Notes:
Emerson & Cuming 11 Eccobond® Heat Cure CatalystGeneral purpose, low viscosity, elevated temperature curing. Long working life. Yields cured coatings with excellent chemical resistance. Subject to partial crystallization at temperatures below 65°C. (Crystals can be removed by gently warming to 65°C and maintaining until all crystals have been dissolved) Cure Type: Heat
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
Viscosity 35 - 60 cP

@Temperature 25.0 °C
35 - 60 cP

@Temperature 77.0 °F
Mixed
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 155 °C
311 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Processing Properties Metric English Comments
Cure Time 120 - 240 min

@Temperature 100 °C
2.00 - 4.00 hour

@Temperature 212 °F
240 - 960 min

@Temperature 150 °C
4.00 - 16.0 hour

@Temperature 302 °F
Pot Life >= 240 min

@Temperature 25.0 °C
>= 240 min

@Temperature 77.0 °F
100 grams
Descriptive Properties Value Comments
Color Dark Brown