Material Notes:
WESTLAKE low-density polyethylene EC1550 is used for extrusion-coating applications, especially when increased heat-seal range is needed.Application/UsesFlexible medicalFoilFood packagingFood-contact applicationsLaminatingMedicalPlaying cardsToys/sporting goodsFDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.917 g/cc
0.0331 lb/in³
ASTM D1505
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 11.0 MPa
1600 psi
500mm/min; ASTM D638 Type IV Specimen
Elongation at Break 500 %
500 %
500mm/min; ASTM D638 Type IV Specimen
2% Secant Modulus 0.207 GPa
30.0 ksi
12.7mm/min; ASTM D790
Processing Properties Metric English Comments
Melt Temperature 149 - 166 °C
300 - 330 °F
Descriptive Properties Value Comments
Process Coating
Region US & Canada
Bamberger Polymers Distribution