| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/PET Polyester Blend , Polyester, TP , Polyethylene Terephthalate (PET) |
| Manufacturer | Aclo Compounders |
| Trade Name | Acculoy |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Aclo Acculoy POL062L Polycarbonate PET Alloy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.22 g/cc | 0.0441 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | MD; ASTM D955 |
| Melt Flow | 13 g/10 min | 13 g/10 min | ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 118 | 118 | ASTM D785 |
| Tensile Strength at Break | 58.0 MPa | 8410 psi | ASTM D638 |
| Tensile Strength, Yield | 59.0 MPa | 8560 psi | ASTM D638 |
| Elongation at Break | 150 % | 150 % | ASTM D638 |
| Elongation at Yield | 86 % | 86 % | ASTM D638 |
| Tensile Modulus | 1.700 GPa | 246.5 ksi | ASTM D638 |
| Flexural Strength | 87.01 MPa | 12620 psi | ASTM D790 |
| Flexural Modulus | 2.499 GPa | 362.5 ksi | ASTM D790 |
| Izod Impact, Notched | 12.9 J/cm | 24.2 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 127 °C | 261 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 106 °C | 223 °F |