| Category | Ceramic , Metal , Electronic/Magnetic Alloy |
| Manufacturer | Alliance LLC |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Alliance BIN-40 Bonded (Composite) Magnetic Material.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 4.50 - 5.50 g/cc | 0.163 - 0.199 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 25.0 - 40.0 MPa | 3630 - 5800 psi | |
| Flexural Strength | 60.0 - 80.0 MPa | 8700 - 11600 psi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 60.0 - 80.0 µm/m-°C @Temperature 20.0 °C |
33.3 - 44.4 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
| Maximum Service Temperature, Air | 100 °C | 212 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.00400 - 0.00700 ohm-cm | 0.00400 - 0.00700 ohm-cm | |
| Magnetic Coercive Force, Hc | 3900 Oe | 3900 Oe | |
| 7980 Oe | 7980 Oe | Intrinsic | |
| Magnetic Remanence, Br | 5000 Gauss | 5000 Gauss | |
| Magnetic Maximum Energy Product, BH | 5.0 MGOe | 5.0 MGOe | |
| Curie Temperature | 300 - 470 °C | 572 - 878 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Reversible Temp Coef., Bd | -0.105 %/°C | |
| Reversible Temp Coef., Hd | -0.40 %/°C | |
| Temperature Coefficient, Br | -0.1 %/°C | (20-100°C) |
| Temperature Coefficient, Hci | -0.4 %/°C | (20-100°C) |