Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Capron® 8232G HS 25% Glass-Filled Nylon 6 (Conditioned)  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Capron® 8232G HS 25% Glass-Filled Nylon 6 (Conditioned)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Capron 8232G HS is a heat stabilized, 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resistance to creep under load is excellent along with its chemical resistance to greases, oils and hydrocarbons.Capron 8232G HS is ideally suited for applications such as safety helmet parts, washers, gears, engine and motor parts, chutes, and higher temperature environments.Data provided by Allied Signal.Processing: Max. water content 0.16%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level.Melt Temperature: 250-280 degC (482-536 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) This product can be processed over a wide range of mold temperatures; however, for applications where aesthetics critical, a mold surface temperature of 80-95 degC (176-203 degF) is required. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Back pressure can be utilized to provide uniform melt consistency and reduce trapped air and gas. A maximum of 3.5 bar (50 psi) is recommended to minimize glass fiber breakage. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing. Surface appearance is directly affected by injection rate. Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
(Dry)
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM Data MD (Dry)
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 105 MPa
15200 psi
ASTM data at 5 mm/min.
Flexural Yield Strength 140 MPa
20300 psi
ASTM Data
Flexural Modulus 3.86 GPa
560 ksi
ASTM Data
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
(Dry)
Processing Properties Metric English Comments
Processing Temperature 275 °C
527 °F
See Materials Notes
Mold Temperature 95.0 °C
203 °F
See Materials Notes
Drying Temperature 85.0 °C
185 °F
See Materials Notes
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved