BASF Capron® B100QP Nylon 6 (DAM)  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Capron® B100QP Nylon 6 (DAM)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Volatiles 0.70 %
0.70 %
Extractable
Water Absorption 1.6 %
1.6 %
24 hr.; ISO 62
9.5 %
9.5 %
ISO 62
Moisture Absorption at Equilibrium 0.040 %
0.040 %
ASTM D570
2.7 %
2.7 %
23°C/50% R.H.; ISO 62
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Nitrogen Transmission 14.0 cc-mm/m²-24hr-atm
35.6 cc-mil/100 in²-24hr-atm
cc/m2/day (Thickness not reported)
Carbon Dioxide Transmission 72.8 cc-mm/m²-24hr-atm
185 cc-mil/100 in²-24hr-atm
cc/m2/day (Thickness not reported)
Viscosity Measurement 3.35
3.35
Relative Viscosity (96% SAV)
3.4
3.4
Relative Viscosity (95% SAV)
3.5
3.5
Relative Viscosity (98% SAV)
100
100
Formic Acid; ASTM D789
Mechanical Properties Metric English Comments
Tensile Strength, Yield 80.0 MPa
11600 psi
2 in/min; ASTM D638
Flexural Strength 100 MPa
14500 psi
ASTM D790
Flexural Modulus 2.62 GPa
380 ksi
ASTM D790
Izod Impact, Notched 0.450 J/cm
0.843 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM D3418
220 °C
428 °F
10 K/min
Descriptive Properties Value Comments
Color Natural
Commercial Status (March 2007) Active America
FDA 21 CFR 177.1500
Impact Modified No
Primary Processing Technique Film Extrusion