| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.15 g/cc | 0.0415 lb/in³ | ISO 1183 |
| 0.980 g/cc @Temperature 330 °C |
0.0354 lb/in³ @Temperature 626 °F |
Melt | |
| Water Absorption | 0.30 % | 0.30 % | Similar to ISO 62 |
| Moisture Absorption at Equilibrium | 0.12 % | 0.12 % | Similar to ISO 62 |
| Melt Flow | 11 g/10 min @Load 2.16 kg, Temperature 330 °C |
11 g/10 min @Load 4.76 lb, Temperature 626 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-1/-2 |
| Elongation at Break | 50 % | 50 % | Nominal; ISO 527-1/-2 |
| Elongation at Yield | 6.8 % | 6.8 % | ISO 527-1/-2 |
| Tensile Modulus | 2.40 GPa | 348 ksi | ISO 527-1/-2 |
| Charpy Impact Unnotched | NB | NB | ISO 179/1eU |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
ISO 179/1eU |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
| Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
| Thermal Conductivity | 0.167 W/m-K | 1.16 BTU-in/hr-ft²-°F | Melt |
| Deflection Temperature at 0.46 MPa (66 psi) | 174 °C | 345 °F | ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 159 °C | 318 °F | ISO 75-1/-2 |
| Flammability, UL94 | V-0 @Thickness 1.50 mm |
V-0 @Thickness 0.0591 in |
IEC 60695-11-10 |
| 5VA @Thickness 3.00 mm |
5VA @Thickness 0.118 in |
IEC 60695-11-20 | |
| Oxygen Index | 35 % | 35 % | ISO 4589-1/-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
| Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | IEC 60093 |
| Dielectric Constant | 3.0 @Frequency 100 Hz |
3.0 @Frequency 100 Hz |
IEC 60250 |
| 3.0 @Frequency 1.00e+6 Hz |
3.0 @Frequency 1.00e+6 Hz |
IEC 60250 | |
| Dielectric Strength | 30.0 kV/mm | 762 kV/in | IEC 60243-1 |
| Dissipation Factor | 0.00070 @Frequency 100 Hz |
0.00070 @Frequency 100 Hz |
IEC 60250 |
| 0.0080 @Frequency 1.00e+6 Hz |
0.0080 @Frequency 1.00e+6 Hz |
IEC 60250 | |
| Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 320 - 330 °C | 608 - 626 °F | |
| 330 °C | 626 °F | Injection Molding; ISO 294 | |
| Mold Temperature | 100 °C | 212 °F | Injection Molding; ISO 10724 |
| 120 - 140 °C | 248 - 284 °F | ||
| Ejection Temperature | 165 °C | 329 °F | |
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Availability | Europe | |
| Near East/Africa | ||
| South and Central America | ||
| Eff. thermal diffusivity (m²/s) | 1E-07 | |
| Form | Pellets | |
| Process | Injection Molding |