| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled |
| Manufacturer | DSM Engineering Plastics |
| Trade Name | Akulon® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DSM Akulon® N24-G6 PA6-GF30.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.35 g/cc | 0.0488 lb/in³ | dry; ISO 1183 |
| Water Absorption | 6.3 % | 6.3 % | Sim. To ISO 62 |
| Moisture Absorption | 1.90 % | 1.90 % | Sim. To ISO 62 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 135 MPa | 19600 psi | dry; ISO 527-1/-2 |
| Elongation at Break | 2.4 % | 2.4 % | dry; ISO 527-1/-2 |
| Tensile Modulus | 9.30 GPa | 1350 ksi | dry; ISO 527-1/-2 |
| Charpy Impact Unnotched | 6.20 J/cm² @Temperature 23.0 °C |
29.5 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
| Charpy Impact, Notched | 0.900 J/cm² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 220 °C | 428 °F | 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | dry; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 200 °C | 392 °F | dry; ISO 75-1/-2 |