Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Akulon® S223-HPG5 Impact Modified Nylon 66-25% Glass Reinforced (European Grade) (Cond)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer DSM Engineering Plastics
Trade Name Akulon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Akulon® S223-HPG5 Impact Modified Nylon 66-25% Glass Reinforced (European Grade) (Cond).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier film, stock shapes, convoluted tubes, and monofilament. Akulon XP is a high-productivity, high-performance PA6 grade for film extrusion processes. Medium viscosity, unreinforced or reinforced Akulon grades are used for various injection molding and blow molding applications. Akulon® Ultraflow® is a high-productivity, high-performance PA6 family for molding processes.Key applications for Akulon: Automotive: Intake manifold, Engine, Powertrain, Airbag containers, Exterior trim, Interior trim, Electrical components and connectorsConsumer durables: Power tools, Lawn and garden tools, Small appliances, Sports and leisure equipment, Furniture, Industrial Goods, TransportationE&E: Low voltage switch gear/power distribution, Lighting, Power connectorsFilm: Specialty and barrier filmsInformation provided by DSM.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
(DAM); ISO 1183
Water Absorption 5.5 %
5.5 %
DAM; Sim. to ISO 62
Moisture Absorption at Equilibrium 1.6 %
1.6 %
Humidity Absorption (DAM); Sim. to ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
ISO 527-1/-2
Elongation at Break 5.5 %
5.5 %
ISO 527-1/-2
Tensile Modulus 6.00 GPa
870 ksi
ISO 527-1/-2
Charpy Impact Unnotched 5.00 J/cm²

@Temperature -30.0 °C
23.8 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
10.0 J/cm²

@Temperature 23.0 °C
47.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²

@Temperature -30.0 °C
4.28 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
1.70 J/cm²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
10°C/min (DAM); ISO 11357-1/-3
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 4.6

@Frequency 1e+6 Hz
4.6

@Frequency 1e+6 Hz
IEC 60250
11

@Frequency 100 Hz
11

@Frequency 100 Hz
IEC 60250
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 60243-1
Dissipation Factor 0.10

@Frequency 1e+6 Hz
0.10

@Frequency 1e+6 Hz
IEC 60250
0.14

@Frequency 100 Hz
0.14

@Frequency 100 Hz
IEC 60250
Comparative Tracking Index 500 V
500 V
IEC 60112
Descriptive Properties Value Comments
Heat stabilized or stable to heat Yes
High impact or impact modified Yes
Injection molding Yes
Release Agent Yes
With Fillers Yes
Users viewing this material also viewed the following: