| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant |
| Manufacturer | DSM Engineering Plastics |
| Trade Name | Arnite® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DSM Arnite® TV4 241 SL PBT-GF20 FR(17).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.62 g/cc | 0.0585 lb/in³ | ISO 1183 |
| Water Absorption | 0.30 % | 0.30 % | Sim. To ISO 62 |
| Moisture Absorption | 0.150 % | 0.150 % | Sim. To ISO 62 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 110 MPa | 16000 psi | ISO 527-1/-2 |
| Elongation at Break | 2.5 % | 2.5 % | ISO 527-1/-2 |
| Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527-1/-2 |
| Charpy Impact Unnotched | 4.50 J/cm² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
| 4.50 J/cm² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU | |
| Charpy Impact, Notched | 0.700 J/cm² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
| 0.700 J/cm² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
| Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ISO 75-1/-2 |
| Flammability, UL94 | V-2 @Thickness 0.750 mm |
V-2 @Thickness 0.0295 in |
IEC 60695-11-10 |
| V-0 @Thickness 1.50 mm |
V-0 @Thickness 0.0591 in |
IEC 60695-11-10 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | IEC 60093 |
| Dielectric Constant | 3.7 @Frequency 1.00e+6 Hz |
3.7 @Frequency 1.00e+6 Hz |
IEC 60250 |
| 3.9 @Frequency 100 Hz |
3.9 @Frequency 100 Hz |
IEC 60250 | |
| Dielectric Strength | 27.0 kV/mm | 686 kV/in | IEC 60243-1 |
| Dissipation Factor | 0.0020 @Frequency 100 Hz |
0.0020 @Frequency 100 Hz |
IEC 60250 |
| 0.015 @Frequency 1.00e+6 Hz |
0.015 @Frequency 1.00e+6 Hz |
IEC 60250 | |
| Comparative Tracking Index | 250 V | 250 V | IEC 60112 |