Material Notes:
30% Glass Reinforced, Flame Retardant
Physical Properties Metric English Comments
Density 1.67 g/cc
0.0603 lb/in³
ISO 1183
Water Absorption 0.60 %
0.60 %
Sim. To ISO 62
Moisture Absorption 0.200 %
0.200 %
Sim. To ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 140 MPa
20300 psi
ISO 527-1/-2
Elongation at Break 2.5 %
2.5 %
ISO 527-1/-2
Tensile Modulus 11.0 GPa
1600 ksi
ISO 527-1/-2
Charpy Impact Unnotched 5.00 J/cm²
<br>@Temperature 23.0 °C
23.8 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eU
5.00 J/cm²
<br>@Temperature -30.0 °C
23.8 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
<br>@Temperature 23.0 °C
4.76 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
1.00 J/cm²
<br>@Temperature -30.0 °C
4.76 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 35.0 µm/m-°C
19.4 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
38.9 µin/in-°F
ISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ISO 75-1/-2
Flammability, UL94 V-2
<br>@Thickness 0.750 mm
V-2
<br>@Thickness 0.0295 in
IEC 60695-11-10
V-0
<br>@Thickness 1.60 mm
V-0
<br>@Thickness 0.0630 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Dielectric Constant 3.4
<br>@Frequency 100 Hz
3.4
<br>@Frequency 100 Hz
IEC 60250
3.4
<br>@Frequency 1.00e+6 Hz
3.4
<br>@Frequency 1.00e+6 Hz
IEC 60250
Dissipation Factor 0.0010
<br>@Frequency 100 Hz
0.0010
<br>@Frequency 100 Hz
IEC 60250
0.015
<br>@Frequency 1.00e+6 Hz
0.015
<br>@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 275 V
275 V
IEC 60112