| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Impact Grade |
| Manufacturer | E-Polymers Co. Ltd. |
| Trade Name | TEKAMID® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | E-Polymers TEKAMID® TB120ST Super Tough PA6, DAM.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792 |
| Water Absorption | 0.60 % | 0.60 % | 23°C/24 hr; ASTM D570 |
| Linear Mold Shrinkage | 0.013 cm/cm | 0.013 in/in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 105 | 105 | ASTM D786 |
| Tensile Strength, Yield | 48.0 MPa | 6960 psi | ASTM D638 |
| Elongation at Break | 150 % | 150 % | ASTM D638 |
| Flexural Yield Strength | 45.0 MPa | 6530 psi | ASTM D790 |
| Flexural Modulus | 1.40 GPa | 203 ksi | ASTM D790 |
| Izod Impact, Notched | 9.00 J/cm | 16.9 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | NB @Thickness 3.20 mm |
NB @Thickness 0.126 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Melting Point | 220 °C | 428 °F | ASTM D2133 |
| Deflection Temperature at 0.46 MPa (66 psi) | 135 °C | 275 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ASTM D648 |
| Flammability, UL94 | HB | HB |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Arc Resistance | 180 sec | 180 sec | Tungsten electrode; ASTM D495 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 250 - 270 °C | 482 - 518 °F | |
| Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F |