Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ecomass® 705ZC75 Stainless Steel Filled ABS

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer Ecomass Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ecomass® 705ZC75 Stainless Steel Filled ABS.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Nontoxic Alternative to traditional metals, weighting and balancing applicationsModerate Specific GravityStainless Steel Powder Filled ABSInformation provided by Technical Polymers
Physical Properties Metric English Comments
Specific Gravity 3.00 g/cc
3.00 g/cc
ISO 1183
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
Internal
Mechanical Properties Metric English Comments
Tensile Strength at Break 28.0 MPa
4060 psi
ISO 527
Elongation at Break 2.0 - 4.0 %
2.0 - 4.0 %
ISO 527
Flexural Modulus 5.40 GPa
783 ksi
ISO 178
Izod Impact, Notched (ISO) 7.40 kJ/m²

@Thickness 3.20 mm
3.52 ft-lb/in²

@Thickness 0.126 in
ISO 180-A
Processing Properties Metric English Comments
Melt Temperature 200 - 270 °C
392 - 518 °F
Mold Temperature 55.0 - 70.0 °C
131 - 158 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 2 - 4 hour
2 - 4 hour