| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.41 g/cc | 0.0509 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.200 % @Temperature 23.0 °C |
0.200 % @Temperature 73.4 °F |
50% RH; ISO 960 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 150 MPa | 21800 psi | ISO 527 |
| Elongation at Break | 2.0 % | 2.0 % | ISO 527 |
| Tensile Modulus | 15.0 GPa | 2180 ksi | ISO 527 |
| Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 250 °C | 482 °F | [10 K/min], ISO 11357 |
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | ISO 75 |
| Flammability, UL94 | HB @Thickness 0.750 mm |
HB @Thickness 0.0295 in |
|
| HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | <= 10000 ohm-cm | <= 10000 ohm-cm | IEC 60093 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
| Feed Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Throat |
| Mold Temperature | 90.0 - 120 °C | 194 - 248 °F | |
| Drying Temperature | 120 - 140 °C | 248 - 284 °F | |
| Dry Time | 4.00 hour | 4.00 hour | |
| Moisture Content | <= 0.080 % | <= 0.080 % | ISO 960 |
| Hold Pressure | 60.0 - 100 MPa | 8700 - 14500 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Back Pressure | Low | |
| Injection Speed | Fast |