Material Notes:
Platinum Ink is designed for oxygen sensor applications. This is a pure platinum ink with no inorganic additions to give maximum response to oxygen. It is suitable for firing on to other high temperature ceramic substrates, in particular zirconia. Application: brushing/dipping – not suitable for screen printingSubstrate: stabilized zirconia and other high temperature ceramic substratesInformation provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 78.9 - 79.1 %

@Temperature 700 °C
78.9 - 79.1 %

@Temperature 1290 °F
Viscosity 130 - 2580 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
130 - 2580 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Storage Temperature 20.0 °C
68.0 °F
sealed container
Processing Properties Metric English Comments
Sintering Temperature 1000 - 1300 °C
1830 - 2370 °F
Firing profile should be over 1-2 hrs with 10-20 mins at peak temperature.
Cure Time 10.0 min

@Temperature 125 °C
0.167 hour

@Temperature 257 °F
15.0 min

@Temperature 100 °C
0.250 hour

@Temperature 212 °F
Shelf Life 6.00 Month
6.00 Month