| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, UV Stabilized |
| Manufacturer | LG Chemical |
| Trade Name | LUPOY |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | LG Chemical Lupoy 1302HP-21 Polycarbonate Resin.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
| Water Absorption | 0.32 % @Temperature 23.0 °C |
0.32 % @Temperature 73.4 °F |
equilibrium, 50% RH; ASTM D570 |
| 0.15 % @Temperature 23.0 °C, Time 86400 sec |
0.15 % @Temperature 73.4 °F, Time 24.0 hour |
ASTM D570 | |
| Linear Mold Shrinkage, Flow | 0.00050 - 0.00070 cm/cm | 0.00050 - 0.00070 in/in | ASTM D955 |
| Melt Flow | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 72 | 72 | ASTM D785 |
| Tensile Strength, Ultimate | 66.0 MPa | 9570 psi | ASTM D638 |
| Tensile Strength, Yield | 60.0 MPa | 8700 psi | 50mm/min; ASTM D638 |
| Elongation at Break | 120 % | 120 % | ASTM D638 |
| Elongation at Yield | 6.0 % | 6.0 % | ASTM D638 |
| Tensile Modulus | 2.34 GPa | 340 ksi | ASTM D638 |
| Flexural Yield Strength | 96.0 MPa | 13900 psi | ASTM D790 |
| Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
| Izod Impact, Notched | 7.47 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
14.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
0.25 mm notch; ASTM D256 |
| Izod Impact, Unnotched | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
ASTM D256 |
| Dart Drop, Total Energy | 72.0 J @Thickness 3.20 mm |
53.1 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
| Abrasion | 45 @Load 1.00 kg |
45 @Load 2.20 lb |
[%], CS-10 F wheel, 500 cycles; ASTM D1044 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
| Hot Ball Pressure Test | >= 125 °C | >= 257 °F | IEC 598-1 |
| Deflection Temperature at 0.46 MPa (66 psi) | 142 °C @Thickness 4.00 mm |
288 °F @Thickness 0.157 in |
Annealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 126 °C @Thickness 4.00 mm |
259 °F @Thickness 0.157 in |
Unannealed; ASTM D648 |
| 139 °C @Thickness 4.00 mm |
282 °F @Thickness 0.157 in |
Annealed; ASTM D648 | |
| Vicat Softening Point | 147 °C @Load 5.10 kg |
297 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
| Softening Point | 150 - 200 °C | 302 - 392 °F | melting point per MSDS |
| UL RTI, Electrical | 80.0 °C @Thickness >=0.500 mm |
176 °F @Thickness >=0.0197 in |
|
| 120 °C @Thickness >=1.60 mm |
248 °F @Thickness >=0.0630 in |
||
| 120 °C @Thickness >=2.50 mm |
248 °F @Thickness >=0.0984 in |
||
| 120 °C @Thickness >=3.00 mm |
248 °F @Thickness >=0.118 in |
||
| UL RTI, Mechanical with Impact | 80.0 °C @Thickness >=0.500 mm |
176 °F @Thickness >=0.0197 in |
|
| 105 °C @Thickness >=1.60 mm |
221 °F @Thickness >=0.0630 in |
||
| 105 °C @Thickness >=2.50 mm |
221 °F @Thickness >=0.0984 in |
||
| 110 °C @Thickness >=3.00 mm |
230 °F @Thickness >=0.118 in |
||
| UL RTI, Mechanical without Impact | 80.0 °C @Thickness >=0.500 mm |
176 °F @Thickness >=0.0197 in |
|
| 120 °C @Thickness >=1.60 mm |
248 °F @Thickness >=0.0630 in |
||
| 120 °C @Thickness >=2.50 mm |
248 °F @Thickness >=0.0984 in |
||
| 120 °C @Thickness >=3.00 mm |
248 °F @Thickness >=0.118 in |
||
| Flammability, UL94 | V-2 @Thickness 0.500 mm |
V-2 @Thickness 0.0197 in |
ASTM D635 |
| V-2 @Thickness 1.60 mm |
V-2 @Thickness 0.0630 in |
ASTM D635 | |
| V-2 @Thickness 2.50 mm |
V-2 @Thickness 0.0984 in |
ASTM D635 | |
| V-2 @Thickness 3.00 mm |
V-2 @Thickness 0.118 in |
ASTM D635 | |
| Flash Point | >= 450 °C | >= 842 °F | |
| Oxygen Index | 26 % | 26 % | ASTM D2863 |
| Glow Wire Test | 850 °C @Thickness 2.00 mm, Time 5.00 sec |
1560 °F @Thickness 0.0787 in, Time 0.00139 hour |
IEC 695-2-1 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.586 | 1.586 | ASTM D542 |
| Haze | 0.70 - 1.5 % | 0.70 - 1.5 % | ASTM D1003 |
| Transmission, Visible | 89 % | 89 % | ASTM D1003 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 2.00e+17 ohm-cm | 2.00e+17 ohm-cm | ASTM D257 |
| Dielectric Constant | 3.0 @Frequency 60.0 Hz |
3.0 @Frequency 60.0 Hz |
ASTM D150 |
| Dielectric Strength | 17.0 kV/mm | 432 kV/in | ASTM D149 |
| Dissipation Factor | 0.0010 @Frequency 60.0 Hz |
0.0010 @Frequency 60.0 Hz |
ASTM D150 |
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
| Comparative Tracking Index | 250 V @Thickness 2.00 mm |
250 V @Thickness 0.0787 in |
IEC 112 |
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=1.60 mm |
30 - 60 sec @Thickness >=0.0630 in |
|
| 30 - 60 sec @Thickness >=2.50 mm |
30 - 60 sec @Thickness >=0.0984 in |
||
| 30 - 60 sec @Thickness >=3.00 mm |
30 - 60 sec @Thickness >=0.118 in |
||
| High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 1.60 mm |
>= 120 arcs @Thickness 0.0630 in |
|
| >= 120 arcs @Thickness 2.50 mm |
>= 120 arcs @Thickness 0.0984 in |
||
| >= 120 arcs @Thickness 3.00 mm |
>= 120 arcs @Thickness 0.118 in |
||
| High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Autoignition Temperature | >450°C | |
| Average Extent of Burning | ASTM D635 |