Acrylic Bonding Adhesives and Thermally Conductive BondersLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. On contact with an activator, these no-mix materials cure rapidly at room temperature to a weather-resistant bond.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
Viscosity 500000 - 1.10e+6 cP
500000 - 1.10e+6 cP
at 2.5 RPM
Mechanical Properties Metric English Comments
Tensile Modulus 1.61 GPa
233 ksi
Adhesive Bond Strength 12.4 MPa
1800 psi
Varies with substrates
Thermal Properties Metric English Comments
CTE, linear 71.0 µm/m-°C

@Temperature 20.0 °C
39.4 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.600 W/m-K
4.16 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Glass Transition Temp, Tg 60.0 °C
140 °F
Processing Properties Metric English Comments
Cure Time 5.00 min
0.0833 hour
Fixture time @ 20ºC
240 - 1440 min
4.00 - 24.0 hour
Full Cure Time @ 20ºC
Shelf Life 9.00 Month
9.00 Month
shelf life at 5ºC
Descriptive Properties Value Comments
Color Grey
Gap Fill 0.01 in.
Viscosity Paste