Overview of materials for Nylon 6, 30% Glass Fiber Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Nylon 6, 30% Glass Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.14 - 1.67 g/cc
0.0410 - 0.0603 lb/in³
Average value: 1.36 g/cc Grade Count:665
1.20 - 1.31 g/cc

@Temperature 250 - 270 °C
0.0434 - 0.0473 lb/in³

@Temperature 482 - 518 °F
Average value: 1.27 g/cc Grade Count:3
Filler Content 25.0 - 35.0 %
25.0 - 35.0 %
Average value: 29.8 % Grade Count:126
Water Absorption 0.130 - 9.00 %
0.130 - 9.00 %
Average value: 3.19 % Grade Count:327
1.60 - 2.50 %

@Temperature 70.0 - 70.0 °C
1.60 - 2.50 %

@Temperature 158 - 158 °F
Average value: 1.95 % Grade Count:8
Moisture Absorption at Equilibrium 0.170 - 7.10 %
0.170 - 7.10 %
Average value: 1.85 % Grade Count:250
0.550 - 1.55 %

@Temperature 70.0 - 70.0 °C
0.550 - 1.55 %

@Temperature 158 - 158 °F
Average value: 1.17 % Grade Count:1
0.550 - 1.55 %

@Time 180000 - 1.44e+6 sec
0.550 - 1.55 %

@Time 50.0 - 400 hour
Average value: 1.17 % Grade Count:1
Water Absorption at Saturation 4.50 - 8.20 %
4.50 - 8.20 %
Average value: 6.64 % Grade Count:62
Viscosity 2.60 - 50.0 cP
2.60 - 50.0 cP
Average value: 9.37 cP Grade Count:7
30.0 - 500 cP

@Temperature 230 - 270 °C
30.0 - 500 cP

@Temperature 446 - 518 °F
Average value: 188 cP Grade Count:2
30.0 - 500 cP

@Shear Rate 100 - 10000 1/s
30.0 - 500 cP

@Shear Rate 100 - 10000 1/s
Average value: 188 cP Grade Count:2
Viscosity Test 104 - 195 cm³/g
104 - 195 cm³/g
Average value: 143 cm³/g Grade Count:30
Maximum Moisture Content 0.100
0.100
Average value: 0.100 Grade Count:42
Linear Mold Shrinkage 0.000300 - 0.0350 cm/cm
0.000300 - 0.0350 in/in
Average value: 0.00417 cm/cm Grade Count:497
0.00280 - 0.00400 cm/cm

@Temperature 80.0 - 80.0 °C
0.00280 - 0.00400 in/in

@Temperature 176 - 176 °F
Average value: 0.00304 cm/cm Grade Count:20
Linear Mold Shrinkage, Transverse 0.000900 - 0.0170 cm/cm
0.000900 - 0.0170 in/in
Average value: 0.00846 cm/cm Grade Count:200
0.00600 - 0.00800 cm/cm

@Temperature 80.0 - 80.0 °C
0.00600 - 0.00800 in/in

@Temperature 176 - 176 °F
Average value: 0.00695 cm/cm Grade Count:20
Melt Flow 1.00 - 101 g/10 min
1.00 - 101 g/10 min
Average value: 30.6 g/10 min Grade Count:88
Spiral Flow 50.0 - 715 cm
19.7 - 281 in
Average value: 102 cm Grade Count:20
Ash 30.0 - 33.1 %
30.0 - 33.1 %
Average value: 31.2 % Grade Count:5
Mechanical Properties Metric English Comments
Hardness, Rockwell L 111 - 115
111 - 115
Average value: 113 Grade Count:10
Hardness, Rockwell M 95.0 - 100
95.0 - 100
Average value: 97.2 Grade Count:5
Hardness, Rockwell R 90.0 - 122
90.0 - 122
Average value: 119 Grade Count:124
Hardness, Shore D 67.0 - 94.0
67.0 - 94.0
Average value: 85.0 Grade Count:31
Ball Indentation Hardness 70.0 - 230 MPa
10200 - 33400 psi
Average value: 169 MPa Grade Count:52
Tensile Strength, Ultimate 28.0 - 203 MPa
4060 - 29500 psi
Average value: 140 MPa Grade Count:477
20.0 - 283 MPa

@Temperature -40.0 - 150 °C
2900 - 41000 psi

@Temperature -40.0 - 302 °F
Average value: 104 MPa Grade Count:19
80.0 - 150 MPa

@Temperature 70.0 - 175 °C
11600 - 21800 psi

@Temperature 158 - 347 °F
Average value: 104 MPa Grade Count:3
80.0 - 150 MPa

@Time 180000 - 7.20e+7 sec
11600 - 21800 psi

@Time 50.0 - 20000 hour
Average value: 104 MPa Grade Count:3
30.0 - 170 MPa

@Strain 1.00 - 2.00 %
4350 - 24700 psi

@Strain 1.00 - 2.00 %
Average value: 104 MPa Grade Count:1
30.0 - 170 MPa

@Temperature -20.0 - 150 °C
4350 - 24700 psi

@Temperature -4.00 - 302 °F
Average value: 104 MPa Grade Count:1
Tensile Strength, Yield 40.0 - 193 MPa
5800 - 28000 psi
Average value: 149 MPa Grade Count:190
111 - 214 MPa

@Temperature -40.0 - 80.0 °C
16100 - 31000 psi

@Temperature -40.0 - 176 °F
Average value: 176 MPa Grade Count:2
Elongation at Break 1.00 - 142 %
1.00 - 142 %
Average value: 4.42 % Grade Count:565
2.50 - 12.0 %

@Temperature -40.0 - 150 °C
2.50 - 12.0 %

@Temperature -40.0 - 302 °F
Average value: 5.91 % Grade Count:12
Elongation at Yield 2.00 - 22.0 %
2.00 - 22.0 %
Average value: 4.17 % Grade Count:93
4.60 - 7.60 %

@Temperature 60.0 - 150 °C
4.60 - 7.60 %

@Temperature 140 - 302 °F
Average value: 5.99 % Grade Count:2
Modulus of Elasticity 1.00 - 15.0 GPa
145 - 2180 ksi
Average value: 7.98 GPa Grade Count:413
2.50 - 11.87 GPa

@Temperature -40.0 - 150 °C
363 - 1722 ksi

@Temperature -40.0 - 302 °F
Average value: 5.80 GPa Grade Count:16
7.00 - 9.00 GPa

@Temperature 70.0 - 70.0 °C
1020 - 1310 ksi

@Temperature 158 - 158 °F
Average value: 5.80 GPa Grade Count:1
7.00 - 9.00 GPa

@Time 180000 - 1.44e+6 sec
1020 - 1310 ksi

@Time 50.0 - 400 hour
Average value: 5.80 GPa Grade Count:1
Flexural Yield Strength 46.0 - 301 MPa
6670 - 43600 psi
Average value: 216 MPa Grade Count:455
89.0 - 380 MPa

@Temperature -40.0 - 121 °C
12900 - 55100 psi

@Temperature -40.0 - 250 °F
Average value: 186 MPa Grade Count:9
Flexural Modulus 0.724 - 14.3 GPa
105 - 2070 ksi
Average value: 7.53 GPa Grade Count:487
2.97 - 12.5 GPa

@Temperature -40.0 - 121 °C
431 - 1810 ksi

@Temperature -40.0 - 250 °F
Average value: 5.07 GPa Grade Count:10
Compressive Yield Strength 140 - 222 MPa
20300 - 32200 psi
Average value: 166 MPa Grade Count:11
Poissons Ratio 0.350
0.350
Average value: 0.350 Grade Count:8
Fatigue Strength >= 54.0 MPa

@Temperature 80.0 - 120 °C
>= 7830 psi

@Temperature 176 - 248 °F
Average value: 61.7 MPa Grade Count:1
>= 54.0 MPa

@Time 0.000 - 374000 sec
>= 7830 psi

@Time 0.000 - 104 hour
Average value: 61.7 MPa Grade Count:1
Shear Modulus 1.32 - 4.10 GPa
191 - 595 ksi
Average value: 2.61 GPa Grade Count:8
>= 0.383 GPa

@Temperature -50.0 - 200 °C
>= 55.6 ksi

@Temperature -58.0 - 392 °F
Average value: 1.13 GPa Grade Count:4
Izod Impact, Notched 0.400 - 3.36 J/cm
0.749 - 6.30 ft-lb/in
Average value: 1.27 J/cm Grade Count:254
0.700 - 3.84408 J/cm

@Temperature -40.0 - 121 °C
1.31 - 7.20154 ft-lb/in

@Temperature -40.0 - 250 °F
Average value: 1.20 J/cm Grade Count:8
1.01441 - 1.33475 J/cm

@Temperature -40.0 - -40.0 °C
1.90041 - 2.50053 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 1.20 J/cm Grade Count:7
Users viewing this material also viewed the following: