Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PlastxWorld DAICEL STYROL® GH10 HIPS

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer PlastxWorld, Inc.
Trade Name DAICEL STYROL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld DAICEL STYROL® GH10 HIPS.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High heat resistance and flame retarded HIPS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Water Absorption 0.10 %
0.10 %
24 hr; ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
Melt Flow 8.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
8.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell L 84
84
ASTM D785
Tensile Strength at Break 21.4 MPa
3100 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Flexural Yield Strength 34.5 MPa
5000 psi
ASTM D790
Flexural Modulus 2.05 GPa
298 ksi
ASTM D790
Izod Impact, Notched 0.961 J/cm

@Thickness 3.17 mm
1.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
0.25 inch; ASTM D648
Vicat Softening Point 97.0 °C
207 °F
ASTM D1525
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Users viewing this material also viewed the following: