Material Notes:
PLENCO 02482 is a general purpose, organic filled phenolic molding compound offering excellent mechanical strength while maintaining dielectric properties at elevated humidity levels. UL recognized under component file E40654. 02482 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.650 g/cc
0.0235 lb/in³
ASTM D1895
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
Water Absorption 0.291 %
0.291 %
ASTM D570
Linear Mold Shrinkage 0.0057 cm/cm
0.0057 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 87
87
ASTM D785
Tensile Strength, Ultimate 59.0 MPa
8560 psi
ASTM D638
Elongation at Break 0.82 %
0.82 %
ASTM D638
Tensile Modulus 8.50 GPa
1230 ksi
ASTM D638
Flexural Strength 94.0 MPa
13600 psi
ASTM D790
Flexural Modulus 8.10 GPa
1170 ksi
ASTM D790
Compressive Strength 206 MPa
29900 psi
ASTM D695
Izod Impact, Notched 0.184 J/cm
0.345 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.198 J/cm²
0.942 ft-lb/in²
ASTM D256
Impact 98
98
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C

@Temperature 40.0 - 130 °C
38.9 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.400 W/m-K

@Temperature 100 °C
2.78 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 206 °C
403 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 168 °C
334 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Oxygen Index 27.2 %
27.2 %
ASTM D2863
Shrinkage 0.21 %
0.21 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
ASTM D247
Dielectric Constant 5.1
5.1
ASTM D150
Dielectric Strength 11.4 kV/mm
290 kV/in
Short Time; ASTM D149
Dissipation Factor 0.053
0.053
ASTM D150
Arc Resistance 132 sec
132 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638