| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled |
| Manufacturer | PolyOne Corporation |
| Trade Name | Bergadur™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Bergadur™ PB400 G10 H UF UV Polybutylene Terephthalate (PBT).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.38 g/cc | 1.38 g/cc | ±0.02; ISO 1183 |
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0090 cm/cm | 0.0040 - 0.0090 in/in | Bergmann method; ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | >= 60.0 MPa @Thickness 4.00 mm, Temperature 23.0 °C |
>= 8700 psi @Thickness 0.157 in, Temperature 73.4 °F |
Injection Molded; ISO 527-2 |
| Elongation at Break | >= 3.0 % @Thickness 4.00 mm, Temperature 23.0 °C |
>= 3.0 % @Thickness 0.157 in, Temperature 73.4 °F |
Injection Molded; ISO 527-2 |
| Tensile Modulus | 4.70 GPa @Thickness 4.00 mm, Temperature 23.0 °C |
682 ksi @Thickness 0.157 in, Temperature 73.4 °F |
Injection Molded; ISO 527-2 |
| Charpy Impact Unnotched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
Injection Molded; ISO 179 |
| Charpy Impact, Notched | 0.420 J/cm² @Temperature 23.0 °C |
2.00 ft-lb/in² @Temperature 73.4 °F |
Injection Molded; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Flammability, UL94 | V-0 @Thickness 1.60 mm |
V-0 @Thickness 0.0630 in |
UL 94 |
| V-0 @Thickness 3.00 mm |
V-0 @Thickness 0.118 in |
UL 94 | |
| Glow Wire Test | 960 °C @Thickness 0.800 mm |
1760 °F @Thickness 0.0315 in |
Flammability Index; IEC 60695-2-12 |
| 960 °C @Thickness 1.50 mm |
1760 °F @Thickness 0.0591 in |
Flammability Index; IEC 60695-2-12 | |
| 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
Flammability Index; IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | ASTM D257 |
| Comparative Tracking Index | 600 V | 600 V | UL 746 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 260 - 280 °C | 500 - 536 °F | |
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
| Drying Temperature | 120 °C | 248 °F | |
| Dry Time | 4.00 hour | 4.00 hour |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | UV Stabilizer | |
| Appearance | Natural Color | |
| Features | Flame Retardant | |
| Halogen Free | ||
| Filler / Reinforcement | Glass Fiber Reinforcement, 10% Filler by Weight | |
| Forms | Pellets | |
| Generic Material | PBT | |
| Generic Name | Polybutylene Terephthalate (PBT) | |
| Regional Availability | Europe |