| Category | Polymer , Thermoplastic , Nylon , Nylon 6 |
| Manufacturer | PolyOne Corporation |
| Trade Name | Bergamid™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Bergamid™ B700 UF V2 Polyamide 6 (Nylon 6).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.13 g/cc | 0.0408 lb/in³ | ±0.03 g/cm³; DIN 53479 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 80.0 MPa @Temperature 23.0 °C |
11600 psi @Temperature 73.4 °F |
ISO 527-2/50 |
| Elongation at Yield | 4.0 % @Temperature 23.0 °C |
4.0 % @Temperature 73.4 °F |
ISO 527-2/50 |
| Tensile Modulus | 3.00 GPa @Temperature 23.0 °C |
435 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
| Charpy Impact Unnotched | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
ISO 179 |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
ISO 179 | |
| Charpy Impact, Notched | 0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
| 0.500 J/cm² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 223 °C | 433 °F | ISO 3146 |
| Maximum Service Temperature, Air | 75.0 °C | 167 °F | Continuous (GTP 50% Tensile); IEC 60216 |
| 175 °C | 347 °F | Short Time; IEC 60216 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 170 °C | 338 °F | Unannealed; ISO 75-2/B |
| Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | Unannealed; ISO 75-2/A |
| Flammability, UL94 | V-2 @Thickness 0.800 mm |
V-2 @Thickness 0.0315 in |
ALL; UL 94 |
| V-2 @Thickness 1.60 mm |
V-2 @Thickness 0.0630 in |
UL 94 | |
| V-2 @Thickness 3.00 mm |
V-2 @Thickness 0.118 in |
UL 94 | |
| Glow Wire Test | 960 °C @Thickness 0.800 mm |
1760 °F @Thickness 0.0315 in |
Flammability Index; IEC 60695-2-12 |
| 960 °C @Thickness 1.60 mm |
1760 °F @Thickness 0.0630 in |
Flammability Index; IEC 60695-2-12 | |
| 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
Flammability Index; IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Flame Retardant | |
| Forms | Pellets | |
| Generic Material | Nylon 6 | |
| Generic Name | Polyamide 6 (Nylon 6) | |
| Processing Method | Injection Molding | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| RoHS Compliance | RoHS Compliant |