| Category | Polymer , Thermoplastic , Acetal (POM) |
| Manufacturer | |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Edgetek® ATH-25GF/000 Acetal-Homopolymer, Glass Filled
(discontinued **).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.59 g/cc | 1.59 g/cc | ASTM D792 |
| Water Absorption | 0.13 % | 0.13 % | 24 hr. Immersion; ASTM D570 |
| Linear Mold Shrinkage | 0.0045 cm/cm | 0.0045 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 94.5 MPa | 13700 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
| Elongation at Yield | 3.0 % | 3.0 % | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
| Tensile Modulus | 8.96 GPa | 1300 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
| Flexural Strength | 115.5 MPa | 16750 psi | ASTM D790 |
| Flexural Modulus | 6.76 GPa | 980 ksi | ASTM D790 |
| Izod Impact, Notched | 1.07 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
2.00 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 45.0 µm/m-°C @Temperature 20.0 °C |
25.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Thermal Conductivity | >= 0.303 W/m-K | >= 2.10 BTU-in/hr-ft²-°F | ASTM C177 |
| Deflection Temperature at 0.46 MPa (66 psi) | 171 °C | 340 °F | Unannealed, 0.125 in bars; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | Unannealed, 0.125 in bars; ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
| Surface Resistivity per Square | 1.00e+14 ohm | 1.00e+14 ohm | ASTM D257 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 199 - 216 °C | 390 - 420 °F | Molding |
| Mold Temperature | 82.2 - 107 °C | 180 - 225 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Product Form | Pellets |