| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded |
| Manufacturer | Polykemi AB |
| Trade Name | POLYabs |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Polykemi AB POLYabs HH0 ABS, Extra Heat Resistance.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.06 g/cc | 0.0383 lb/in³ | ISO 1183 |
| Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | With Flow; ISO 2577 |
| 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | Across Flow; ISO 2577 | |
| Melt Index of Compound | 5.0 g/10 min @Load 5.00 kg, Temperature 230 °C |
5.0 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | <= 48.0 MPa | <= 6960 psi | ISO/R527 |
| Elongation at Yield | 6.0 % | 6.0 % | ISO/R527 |
| Flexural Strength | <= 85.0 MPa | <= 12300 psi | ISO 178 |
| Flexural Modulus | 2.50 GPa @Temperature 23.0 °C |
363 ksi @Temperature 73.4 °F |
ISO 178 |
| Charpy Impact, Notched | 0.800 J/cm² @Temperature -20.0 °C |
3.81 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
| 1.10 J/cm² @Temperature 23.0 °C |
5.23 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 219 °F | 120°C/h; ISO 75/1 |
| Deflection Temperature at 1.8 MPa (264 psi) | 90.0 °C | 194 °F | 120°C/h; ISO 75/1 |
| Vicat Softening Point | 115 °C @Load 5.001 kg |
239 °F @Load 11.03 lb |
50°C/h; ISO 306 |
| 134 °C @Load 1.00 kg |
273 °F @Load 2.21 lb |
50°C/h; ISO 306 | |
| Flammability, UL94 | HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 190 - 230 °C | 374 - 446 °F | |
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
| Drying Temperature | 80.0 °C | 176 °F | |
| Dry Time | 2 - 4 hour | 2 - 4 hour | in circulation dryer |
| 2 - 4 hour | 2 - 4 hour | in fresh-air dryer | |
| 2 - 4 hour | 2 - 4 hour | in desiccant air dryer | |
| Injection Pressure | 90.0 - 150 MPa | 13100 - 21800 psi | |
| Back Pressure | 1.00 - 1.50 MPa | 145 - 218 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Holding Pressure () | 20-40 | % of injection pressure |
| Injection Speed () | High |