Polyram RamTough PZ300G8 Polycarbonate, 40% Glass Fiber

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 40% Glass Filled
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Polyram RamTough PZ300G8 Polycarbonate, 40% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
40% Glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
DIN 53479
Water Absorption 0.070 %
0.070 %
DIN 53495
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
Melt Flow 10 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
10 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 130 MPa
18900 psi
ASTM-D638
Elongation at Break 2.0 %
2.0 %
ASTM-D638
Flexural Strength 195 MPa
28300 psi
ASTM D790
Flexural Modulus 7.00 GPa
1020 ksi
ASTM-D790
Izod Impact, Notched 1.50 J/cm
<br>@Temperature 23.0 °C
2.81 ft-lb/in
<br>@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
DIN 52612
Deflection Temperature at 0.46 MPa (66 psi) 147 °C
297 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 139 °C
282 °F
DIN 53461
Flammability, UL94 V-1
<br>@Thickness 3.00 mm
V-1
<br>@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
DIN 53482
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
DIN 53482
Dielectric Constant 3.3
<br>@Frequency 1e+6 Hz
3.3
<br>@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 30.0 kV/mm
762 kV/in
VDE 0303/4