Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radilon® S RCV3015 (cond.) Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Radici Radilon® S RCV3015 (cond.) Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
(Dry)
Water Absorption 7.9 %
7.9 %
initially dry
Moisture Absorption at Equilibrium 2.2 %
2.2 %
initially dry
Viscosity Measurement 140
140
cm³/g Viscosity Number
Mechanical Properties Metric English Comments
Tensile Strength, Yield 85.0 MPa
12300 psi
Elongation at Break 9.5 %
9.5 %
Nominal
Elongation at Yield 3.9 %
3.9 %
Tensile Modulus 6.10 GPa
885 ksi
Charpy Impact Unnotched 3.80 J/cm²
<br>@Temperature -30.0 °C
18.1 ft-lb/in²
<br>@Temperature -22.0 °F
7.00 J/cm²
<br>@Temperature 23.0 °C
33.3 ft-lb/in²
<br>@Temperature 73.4 °F
Charpy Impact, Notched 0.430 J/cm²
<br>@Temperature -30.0 °C
2.05 ft-lb/in²
<br>@Temperature -22.0 °F
0.850 J/cm²
<br>@Temperature 23.0 °C
4.04 ft-lb/in²
<br>@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
(Dry)
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 550 V
550 V
Copyright © lookpolymers.com All Rights Reserved