| Category | Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Cycoloy® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics Cycoloy® CE3510 PC+ABS (Europe-Africa-Middle East).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
| Density | 1.21 g/cc | 0.0437 lb/in³ | ISO 1183 |
| Melt Index of Compound | 8.0 g/10 min @Load 5.00 kg, Temperature 260 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 49.0 MPa | 7110 psi | Type I, 50 mm/min; ASTM D638 |
| 50.0 MPa | 7250 psi | 50 mm/min; ISO 527 | |
| Tensile Strength, Yield | 64.0 MPa | 9280 psi | Type I, 50 mm/min; ASTM D638 |
| 65.0 MPa | 9430 psi | 50 mm/min; ISO 527 | |
| Elongation at Break | 35 % | 35 % | Type I, 50 mm/min; ASTM D638 |
| >= 50 % | >= 50 % | 50 mm/min; ISO 527 | |
| Elongation at Yield | 4.3 % | 4.3 % | Type I, 50 mm/min; ASTM D638 |
| 4.6 % | 4.6 % | 50 mm/min; ISO 527 | |
| Tensile Modulus | 2.68 GPa | 389 ksi | 50 mm/min; ASTM D638 |
| Flexural Yield Strength | 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 95.0 MPa | 13800 psi | 2 mm/min; ISO 178 | |
| Flexural Modulus | 2.47 GPa | 358 ksi | 2 mm/min; ISO 178 |
| 2.61 GPa | 379 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Izod Impact, Notched | 6.64 J/cm | 12.4 ft-lb/in | ASTM D256 |
| 1.09 J/cm @Temperature -30.0 °C |
2.04 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
| Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1A |
| 54.0 kJ/m² | 25.7 ft-lb/in² | 80*10*3; ISO 180/1A | |
| 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A | |
| 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
| 14.0 kJ/m² @Temperature 0.000 °C |
6.66 ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A | |
| Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
| 1.20 J/cm² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 111 °C | 232 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
| 111 °C @Thickness 3.20 mm |
232 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
| 100 °C @Thickness 3.20 mm |
212 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 116 °C | 241 °F | Rate B/50; ISO 306 |
| 118 °C | 244 °F | Rate B/120; ISO 306 | |
| Flammability, UL94 | V-2 @Thickness 0.750 mm |
V-2 @Thickness 0.0295 in |
UL 94 |
| V-0 @Thickness 1.50 mm |
V-0 @Thickness 0.0591 in |
UL 94 | |
| Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
| 825 °C | 1520 °F | IEC 60695-2-13 | |
| 825 °C | 1520 °F | IEC 60695-2-13 | |
| 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
| 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 | |
| 44.0 kV/mm @Thickness 0.800 mm |
1120 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Ball Pressure Test, 75°C +/- 2°C | PASSES | IEC 60695-10-2 |