| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
| Melt Flow | 14 g/10 min @Load 5.00 kg, Temperature 260 °C |
14 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 62.0 MPa | 8990 psi | Type I, 50 mm/min; ASTM D638 |
| Tensile Strength, Yield | 64.0 MPa | 9280 psi | Type I, 50 mm/min; ASTM D638 |
| Elongation at Break | 85 % | 85 % | Type I, 50 mm/min; ASTM D638 |
| >= 100 % | >= 100 % | 50 mm/min; ISO 527 | |
| Elongation at Yield | 5.7 % | 5.7 % | 50 mm/min; ISO 527 |
| 6.0 % | 6.0 % | Type I, 50 mm/min; ASTM D638 | |
| Tensile Modulus | 2.33 GPa | 338 ksi | 5 mm/min; ASTM D638 |
| Izod Impact, Notched | 7.95 J/cm | 14.9 ft-lb/in | ASTM D256 |
| 2.15 J/cm @Temperature -30.0 °C |
4.03 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
| 5.25 J/cm @Temperature 0.000 °C |
9.84 ft-lb/in @Temperature 32.0 °F |
ASTM D256 | |
| Charpy Impact, Notched | 2.80 J/cm² | 13.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
| 1.20 J/cm² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA | |
| 1.70 J/cm² @Temperature 0.000 °C |
8.09 ft-lb/in² @Temperature 32.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
| CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 118 °C @Thickness 6.40 mm |
244 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
| Vicat Softening Point | 133 °C | 271 °F | Rate B/50; ISO 306 |
| 134 °C | 273 °F | Rate B/120; ISO 306 | |
| Flammability, UL94 | V-0 @Thickness 1.20 mm |
V-0 @Thickness 0.0472 in |
UL 94 |
| 5VB @Thickness 2.50 mm |
5VB @Thickness 0.0984 in |
UL 94 | |
| Oxygen Index | 32 % | 32 % | ISO 4589 |
| Glow Wire Test | 775 °C | 1430 °F | IEC 60695-2-13 |
| 775 °C | 1430 °F | IEC 60695-2-13 | |
| 775 °C | 1430 °F | IEC 60695-2-13 | |
| 960 °C @Thickness 0.750 mm |
1760 °F @Thickness 0.0295 in |
IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | >= 4.00e+16 ohm | >= 4.00e+16 ohm | ROA; IEC 60093 |
| Dielectric Constant | 2.95 @Frequency 1.00e+6 Hz |
2.95 @Frequency 1.00e+6 Hz |
ASTM D150 |
| 3.01 @Frequency 1000 Hz |
3.01 @Frequency 1000 Hz |
ASTM D150 | |
| Dissipation Factor | 0.0017 @Frequency 1000 Hz |
0.0017 @Frequency 1000 Hz |
ASTM D150 |
| 0.0088 @Frequency 1.00e+6 Hz |
0.0088 @Frequency 1.00e+6 Hz |
ASTM D150 | |
| 0.0088 @Frequency 1.00e+6 Hz |
0.0088 @Frequency 1.00e+6 Hz |
IEC 60250 | |
| Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
| Hot Wire Ignition, HWI | 30 - 60 sec | 30 - 60 sec | UL 746A |
| High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL 746A |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Ball Pressure Test, 125°C +/- 2°C | Pass | IEC 60695-10-2 |
| Ball Pressure Test, 125°C +/- 2°C, by VDE | Pass | IEC 60695-10-2 |