| Category | Polymer , Thermoplastic , ASA Polymer |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | GELOY |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics GELOY CR7520 ASA (Asia Pacific).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | ASTM D792 |
| Moisture Absorption at Equilibrium | 0.55 % | 0.55 % | ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 7.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
| 13 g/10 min @Load 5.00 kg, Temperature 260 °C |
13 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 86 | 86 | ASTM D785 |
| Tensile Strength at Break | 34.0 MPa | 4930 psi | Type I, 50 mm/min; ASTM D638 |
| Tensile Strength, Yield | 41.0 MPa | 5950 psi | Type I, 50 mm/min; ASTM D638 |
| Elongation at Break | 40 % | 40 % | Type I, 50 mm/min; ASTM D638 |
| Tensile Modulus | 1.79 GPa | 260 ksi | 50 mm/min; ASTM D638 |
| Flexural Yield Strength | 58.0 MPa | 8410 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Flexural Modulus | 1.79 GPa | 260 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Izod Impact, Notched | 3.20 J/cm | 5.99 ft-lb/in | ASTM D256 |
| 0.580 J/cm @Temperature -30.0 °C |
1.09 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
| Dart Drop, Total Energy | 25.0 J @Temperature 23.0 °C |
18.4 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 84.6 µm/m-°C @Temperature -30.0 - 0.000 °C |
47.0 µin/in-°F @Temperature -22.0 - 32.0 °F |
ASTM E 831 |
| 86.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 | |
| 90.0 µm/m-°C @Temperature 0.000 - 100 °C |
50.0 µin/in-°F @Temperature 32.0 - 212 °F |
ASTM E 831 | |
| CTE, linear, Transverse to Flow | 91.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C @Thickness 3.20 mm |
189 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| 90.0 °C @Thickness 6.40 mm |
194 °F @Thickness 0.252 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C | 203 °F | annealed; ASTM D648 |
| 76.0 °C @Thickness 3.20 mm |
169 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| 79.0 °C @Thickness 6.40 mm |
174 °F @Thickness 0.252 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 99.0 °C | 210 °F | Rate B/50; ASTM D1525 |
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
| UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746B |
| UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
| Flammability, UL94 | HB @Thickness 1.47 mm |
HB @Thickness 0.0579 in |
UL 94 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Gloss | 95 % | 95 % | untextured, 60 degrees; ASTM D523 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
| Dielectric Constant | 3.21 @Frequency 1.00e+6 Hz |
3.21 @Frequency 1.00e+6 Hz |
ASTM D150 |
| 5.2 @Frequency 50.0 - 60.0 Hz |
5.2 @Frequency 50.0 - 60.0 Hz |
ASTM D150 | |
| Dielectric Strength | 15.9 kV/mm @Thickness 3.20 mm |
404 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
| Dissipation Factor | 0.026 @Frequency 1.00e+6 Hz |
0.026 @Frequency 1.00e+6 Hz |
ASTM D150 |
| 0.15 @Frequency 50.0 - 60.0 Hz |
0.15 @Frequency 50.0 - 60.0 Hz |
ASTM D150 | |
| Comparative Tracking Index | >= 600 V | >= 600 V | UL 746A |
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
| High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
| Descriptive Properties | Value | Comments |
|---|---|---|
| UV-light, water exposure/immersion | F2 | UL 746C |