| Category | Polymer , Thermoplastic , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Lexan® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics Lexan® LGK4030 PC (Asia Pacific).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.54 g/cc | 1.54 g/cc | ASTM D792 |
| Water Absorption | 0.14 % @Time 86400 sec |
0.14 % @Time 24.0 hour |
ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0015 - 0.0020 cm/cm @Thickness 3.20 mm |
0.0015 - 0.0020 in/in @Thickness 0.126 in |
SABIC Method |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 91 | 91 | ASTM D785 |
| Tensile Strength, Yield | 129 MPa | 18700 psi | SABIC - Japan Method |
| Elongation at Break | 3.0 - 5.0 % | 3.0 - 5.0 % | SABIC - Japan Method |
| Flexural Strength | 180 MPa | 26100 psi | ASTM D790 |
| Flexural Modulus | 8.82 GPa | 1280 ksi | ASTM D790 |
| Izod Impact, Notched | 1.07 J/cm | 2.00 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 22.0 - 43.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
12.2 - 23.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
| Deflection Temperature at 0.46 MPa (66 psi) | 145 °C @Thickness 3.20 mm |
293 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |