| Category | Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Noryl |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics NORYL 115 PPE+HIPS (Asia Pacific).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
| Water Absorption | 0.070 % @Time 86400 sec |
0.070 % @Time 24.0 hour |
ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 13.2 g/10 min @Load 10.0 kg, Temperature 250 °C |
13.2 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | SABIC - Japan Method |
| Elongation at Break | 75 % | 75 % | SABIC - Japan Method |
| Flexural Strength | 68.0 MPa | 9860 psi | ASTM D790 |
| Flexural Modulus | 2.15 GPa | 312 ksi | ASTM D790 |
| Izod Impact, Notched | 1.56 J/cm | 2.92 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 65.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
36.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
| Deflection Temperature at 1.8 MPa (264 psi) | 115 °C @Thickness 6.40 mm |
239 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
| Flammability, UL94 | HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
UL 94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
| Dielectric Constant | 2.7 @Frequency 50.0 - 60.0 Hz |
2.7 @Frequency 50.0 - 60.0 Hz |
ASTM D150 |