| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Valox® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics Valox® IQ3001 PBT (Europe-Africa-Middle East).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
| Density | 1.31 g/cc | 0.0473 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.0700 % | 0.0700 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.11 % | 0.11 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.021 - 0.027 cm/cm @Thickness 3.20 mm |
0.021 - 0.027 in/in @Thickness 0.126 in |
SABIC Method |
| Linear Mold Shrinkage, Transverse | 0.021 - 0.027 cm/cm @Thickness 3.20 mm |
0.021 - 0.027 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 26 g/10 min @Load 1.20 kg, Temperature 250 °C |
26 g/10 min @Load 2.65 lb, Temperature 482 °F |
ASTM D1238 |
| Melt Index of Compound | 24 g/10 min @Load 1.20 kg, Temperature 250 °C |
24 g/10 min @Load 2.65 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 50.0 MPa | 7250 psi | 50 mm/min; ISO 527 |
| 51.0 MPa | 7400 psi | Type I, 50 mm/min; ASTM D638 | |
| Tensile Strength, Yield | 55.0 MPa | 7980 psi | 50 mm/min; ISO 527 |
| 56.0 MPa | 8120 psi | Type I, 50 mm/min; ASTM D638 | |
| Elongation at Break | 60 % | 60 % | Type I, 50 mm/min; ASTM D638 |
| 60 % | 60 % | 50 mm/min; ISO 527 | |
| Elongation at Yield | 5.0 % | 5.0 % | Type I, 50 mm/min; ASTM D638 |
| 5.0 % | 5.0 % | 50 mm/min; ISO 527 | |
| Tensile Modulus | 2.60 GPa | 377 ksi | 5 mm/min; ASTM D638 |
| 2.60 GPa | 377 ksi | 1 mm/min; ISO 527 | |
| Flexural Yield Strength | 80.0 MPa | 11600 psi | 2 mm/min; ISO 178 |
| 82.0 MPa | 11900 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Flexural Modulus | 2.40 GPa | 348 ksi | 2 mm/min; ISO 178 |
| 2.50 GPa | 363 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Izod Impact, Notched | 0.280 J/cm | 0.525 ft-lb/in | ASTM D256 |
| 0.270 J/cm @Temperature -30.0 °C |
0.506 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
| Izod Impact, Unnotched | 17.0 J/cm | 31.8 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
| 4.00 kJ/m² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
| Charpy Impact, Notched | 1.10 J/cm² | 5.23 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| Dart Drop, Total Energy | 23.0 J @Temperature 23.0 °C |
17.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 85.0 µm/m-°C @Temperature -40.0 - 150 °C |
47.2 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
| 85.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
47.2 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature -40.0 - 150 °C |
43.9 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
| 79.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
43.9 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 135 °C | 275 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| 148 °C @Thickness 6.40 mm |
298 °F @Thickness 0.252 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 48.0 °C | 118 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 54.0 °C @Thickness 3.20 mm |
129 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 177 °C | 351 °F | Rate B/50; ASTM D1525 |
| 177 °C | 351 °F | Rate B/120; ISO 306 | |
| 178 °C | 352 °F | Rate B/50; ISO 306 |