Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU)

Category Polymer , Thermoplastic , Polysulfone (PSU)
Manufacturer Solvay Specialty Polymers
Trade Name Udel®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Udel® P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand prolonged exposure to high temperatures and repeated sterilization. Udel® P-1700 polysulfone is highly resistant to mineral acids, alkali and salt solutions. Resistance to detergents and hydrocarbon oils is good, but the resin may be attacked by polar solvents such as ketones, chlorinated hydrocarbons and aromatic hydrocarbons.Features: Acid Resistant; Alcohol Resistant; Alkali Resistant; Autoclave Sterilizable; Biocompatible; Detergent Resistant; E-beam Sterilizable; Ethylene Oxide Sterilizable; Food Contact Acceptable; Good Chemical Resistance; Good Dimensional Stability; Good Sterilizability; Good Surface Finish; Good Toughness; Heat Sterilizable; High Heat Resistance; Hydrocarbon Resistant; Hydrolytically Stable; Radiation (Gamma) Resistant; Radiation Sterilizable; Radiotranslucent; Steam Resistant; Steam SterilizableUses: Appliance Components; Appliances; Automotive Electronics; Dental Applications; Electrical Parts; Electrical/Electronic Applications; Food Service Applications; Hospital Goods; Industrial Parts; Medical Devices; Medical/Healthcare Applications; Microwave Cookware; Piping; Plumbing Parts; Surgical Instruments; Valves/Valve PartsAutomotive Specifications ASTM D6394 SP0112; BMW GS 93016Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Water Absorption 0.30 %

@Time 86400 sec
0.30 %

@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cm
0.0070 in/in
Melt Flow 6.5 g/10 min

@Load 2.16 kg,
Temperature 343 °C
6.5 g/10 min

@Load 4.76 lb,
Temperature 649 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 70.3 MPa
10200 psi
ASTM D638
Elongation at Break 50 - 100 %
50 - 100 %
ASTM D638
Tensile Modulus 2.48 GPa
360 ksi
ASTM D638
Flexural Strength 106 MPa
15400 psi
ASTM D790
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
Tensile Impact Strength 420 kJ/m²
200 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
Deflection Temperature at 1.8 MPa (264 psi) 174 °C
345 °F
Unannealed; ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
V-0

@Thickness 4.50 mm
V-0

@Thickness 0.177 in
Glow Wire Test 850 °C

@Thickness 0.800 mm
1560 °F

@Thickness 0.0315 in
Glow Wire Flammability Index, IEC 60695-2-12
850 °C

@Thickness 1.60 - 6.00 mm
1560 °F

@Thickness 0.0630 - 0.236 in
Glow Wire Ignition Temperature; IEC 60695-2-13
875 °C

@Thickness 0.800 mm
1610 °F

@Thickness 0.0315 in
Glow Wire Ignition Temperature; IEC 60695-2-13
960 °C

@Thickness 1.60 - 6.00 mm
1760 °F

@Thickness 0.0630 - 0.236 in
Glow Wire Flammability Index, IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+16 ohm-cm
3.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.02

@Frequency 1.00e+6 Hz
3.02

@Frequency 1.00e+6 Hz
ASTM D150
3.03

@Frequency 60.0 Hz
3.03

@Frequency 60.0 Hz
ASTM D150
3.04

@Frequency 1000 Hz
3.04

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm
432 kV/in
ASTM D149
Dissipation Factor 0.0010

@Frequency 1000 Hz
0.0010

@Frequency 1000 Hz
ASTM D150
0.0060

@Frequency 1.00e+6 Hz
0.0060

@Frequency 1.00e+6 Hz
ASTM D150
0.0070

@Frequency 60.0 Hz
0.0070

@Frequency 60.0 Hz
ASTM D150
Compliance Properties Metric English Comments
FDA Yes
Yes
NSF Yes
Yes
NSF 51; NSF 61
Processing Properties Metric English Comments
Melt Temperature 329 - 385 °C
624 - 725 °F
Mold Temperature 121 - 163 °C
250 - 325 °F
Drying Temperature 135 - 163 °C

@Time 12600 sec
275 - 325 °F

@Time 3.50 hour
Shot Size 50 - 75 %
50 - 75 %
Descriptive Properties Value Comments
Agency Ratings FDA 21 CFR 177.1655; ISO 10993; ISO 10993-Part 1
Availability Asia Pacific
Europe
Latin America
North America
Color Colors Available; Transparent - Slight Yellow
Form Pellets
Processing Technique Extrusion; Extrusion Blow Molding; Film Extrusion
Injection Blow Molding; Injection Molding
Machining; Pipe Extrusion
Profile Extrusion; Sheet Extrusion; Thermoforming
RoHS Compliance RoHS Compliant
Users viewing this material also viewed the following: