Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill FR® PBT FR

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Flame Retardant , Polybutylene Terephthalate (PBT), Unreinforced, Molded
Manufacturer Techmer ES
Trade Name HiFill FR®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill FR® PBT FR.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
Water Absorption 0.080 %

@Time 86400 sec
0.080 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.025 cm/cm

@Thickness 3.17 mm
0.025 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength 56.5 MPa
8200 psi
ASTM D638
Elongation at Yield 75 %
75 %
ASTM D638
Flexural Yield Strength 101 MPa
14700 psi
ASTM D790
Flexural Modulus 2.62 GPa
380 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm

@Thickness 3.17 mm
0.700 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 72.0 µm/m-°C
40.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C
160 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
ASTM D257
Dielectric Strength 18.1 kV/mm
460 kV/in
Method A (Short-Time); ASTM D149
Users viewing this material also viewed the following: