| Category | Polymer , Thermoplastic , Nylon , Nylon 6/66 |
| Manufacturer | |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Technetics Group Amicon™ Nylon 6/66
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D792 |
| Water Absorption | 0.30 % | 0.30 % | 24 hours; ASTM D570 (2) |
| Water Absorption at Saturation | 7.0 % | 7.0 % | ASTM D570 (2) |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 75.8 MPa | 11000 psi | ASTM D638 |
| Elongation at Break | 50 % | 50 % | ASTM D638 |
| Modulus of Elasticity | 2.76 GPa | 400 ksi | ASTM D638 |
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
| Compressive Strength | 117 MPa | 17000 psi | ASTM D695 |
| Izod Impact, Notched | 0.320 J/cm | 0.600 ft-lb/in | ASTM D256 type "A" |
| Coefficient of Friction | 0.25 | 0.25 | ASTM PTM 55007 |
| K (wear) Factor | 145 x 10<sup>-8</sup> mm³/N-M | 72.0 x 10<sup>-10</sup> in³-min/ft-lb-hr | QTM 55010 |
| Limiting Pressure Velocity | 0.0946 MPa-m/sec | 2700 psi-ft/min | 4:1 safety factor |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 99.0 µm/m-°C @Temperature 100 °C |
55.0 µin/in-°F @Temperature 212 °F |
ASTM E-831 (TMA) |
| Maximum Service Temperature, Air | 98.9 °C | 210 °F | |
| Flammability, UL94 | HB @Thickness 3.17 mm |
HB @Thickness 0.125 in |
ASTM UL-94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 4.1 @Frequency 1e+6 Hz |
4.1 @Frequency 1e+6 Hz |
ASTM D150 |
| Dielectric Strength | 15.7 kV/mm | 400 kV/in | ASTM D149 |