Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Telcar® TL-8712 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name TELCAR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Telcar® TL-8712 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Underground Power Cable; Wire and Cable Applications; Wire Jacketing Wire Types: SJEOW Agency Ratings: UL 1581; QMTT2.E73402 Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C); Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792
Melt Flow 2.00 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.00 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 73
73
ASTM D2240
Tensile Strength at Break 13.5 MPa
1960 psi
ASTM D412
Elongation at Break 680 %
680 %
ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Continuous Use
Oxygen Index 20 %
20 %
ASTM D2863
Processing Properties Metric English Comments
Rear Barrel Temperature 199 - 216 °C
390 - 420 °F
Middle Barrel Temperature 213 - 221 °C
415 - 430 °F
Front Barrel Temperature 221 - 227 °C
430 - 440 °F
Nozzle Temperature 221 - 229 °C
430 - 445 °F
Zone 1 193 - 210 °C
380 - 410 °F
Zone 2 199 - 216 °C
390 - 420 °F
Zone 3 213 - 221 °C
415 - 430 °F
Zone 5 221 - 227 °C
430 - 440 °F
Die Temperature 221 - 229 °C
430 - 445 °F
Melt Temperature 221 - 229 °C
430 - 445 °F
Processing Temperature
Mold Temperature 25.0 - 65.6 °C
77.0 - 150 °F
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Back Pressure 0.172 - 0.345 MPa
25.0 - 50.0 psi
Cushion 0.381 - 2.54 cm
0.150 - 1.00 in
Screw Speed 50 - 100 rpm
50 - 100 rpm
Descriptive Properties Value Comments
Appearance Opaque
Users viewing this material also viewed the following: